Abstract

Results are presented on the hysteretic properties of heat-treated melt-spun Nd13Fe79B8. The influence on the coercive force of the following parameters has been investigated: the proportion of crystalline phases present in the as-quenched material, the heating rate up to the annealing temperature as well as the annealing time and temperature. The set of preparation and treatment parameters leads to a maximum coercive force of 2 T. © 1992.
Original languageEnglish
Pages (from-to)1141-1142
JournalJournal of Magnetism and Magnetic Materials
Volume104-107
Issue numberPART 2
DOIs
Publication statusPublished - 2 Feb 1992

Fingerprint Dive into the research topics of 'Hysteretic behaviour of melt-spun Nd<inf>13</inf>Fe<inf>79</inf>B<inf>8</inf> after different crystallization treatments'. Together they form a unique fingerprint.

Cite this